性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測(cè)試方法 |
測(cè)試數(shù)據(jù) |
數(shù)據(jù)單位 |
基本性能 |
24小時(shí)吸水率 |
--- |
ASTM D-570 |
0.3 |
% |
物理性能 |
泰伯磨耗量 |
CS-17輪 |
ASTM D-1044 |
7 |
mg/1000rev |
比重 |
--- |
ASTM D-792 |
1.22 |
--- |
熔體流動(dòng)速率 |
--- |
ASTM D-1238 |
8.5 |
g/10min |
泰伯磨耗量 |
H 18輪 |
ASTM D-1044 |
77 |
mg/1000rev |
機(jī)械性能 |
硬度計(jì)硬度 |
--- |
ASTM D-2240 |
63 |
--- |
揉曲模量 |
23℃ |
ASTM D-790 |
330 |
Mpa |
斷裂拉伸力 |
--- |
ASTM D-638 |
41 |
Mpa |
斷裂伸長(zhǎng) |
--- |
ASTM D-638 |
420 |
% |
拉伸力 |
5%伸長(zhǎng) |
10%伸長(zhǎng) |
|
--- |
|
|
|
埃佐沖擊強(qiáng)度 |
23℃ |
ASTM D-256 |
不破裂 |
J/m |
初耐撕裂性能 |
--- |
ASTM D-1004 |
175 |
kn/m |
熱 性 能 |
熔點(diǎn) |
--- |
ASTM D-3418 |
211 |
℃ |
維卡軟化點(diǎn) |
--- |
ASTM D-1525 |
95 |
℃ |
熱畸變溫度 |
@0.5Mpa |
ASTM D-648 |
115 |
℃ |
熱畸變溫度 |
@0.18Mpa |
ASTM D-648 |
51 |
℃ |
其它性能 |
耐揉曲切口增長(zhǎng)性能 |
--- |
ASTM D-1052 |
>5×105 |
--- |