規(guī)格 | 壁厚 | 規(guī)格 | 壁厚 | 規(guī)格 | 壁厚 | 規(guī)格 | 壁厚 |
DN15 | 1.8 | DN40 | 1.8 | DN80 | 2.2 | DN150 | 2.5 |
2.0 | 2.0 | 2.5 | 2.75 | ||||
2.2 | 2.2 | 2.75 | 3.0 | ||||
2.5 | 2.5 | 3.0 | 3.25 | ||||
2.75 | 2.75 | 3.25 | 3.5 | ||||
DN20 | 1.8 | 3.0 | 3.5 | 3.75 | |||
2.0 | 3.25 | 3.74 | 4.0 | ||||
2.2 | 3.5 | 4.0 | 4.25 | ||||
2.5 | DN50 | 1.8 | DN100 | 2.0 | DN200 | 2.75 | |
2.75 | 2.0 | 2.2 | 3.0 | ||||
DN25 | 1.8 | 2.2 | 2.5 | 3.25 | |||
2.0 | 2.5 | 2.75 | 3.5 | ||||
2.2 | 2.75 | 3.0 | 3.75 | ||||
2.5 | 3.0 | 3.25 | 4.0 | ||||
2.75 | 3.25 | 3.5 | 4.25 | ||||
3.0 | 3.5 | 3.75 | 4.5 | ||||
3.25 | DN65 | 2.2 | 4.0 | 4.75 | |||
DN32 | 1.8 | 2.5 | 4.25 | 5.0 | |||
2.0 | 2.75 | DN125 | 2.5 | DN200 | 5.5 | ||
2.2 | 3.0 | 2.75 | DN200 | 5.75 | |||
2.5 | 3.25 | 3.0 | DN200 | 6.0 | |||
2.75 | 3.5 | 3.25 | |||||
3.0 | 3.75 | 3.5 | |||||
3.25 | 3.75 | ||||||
4.0 |
鍍鋅管的分類
鍍鋅鋼管分冷鍍管、熱鍍管,前者已被禁用,后者還被國家提倡暫時能用.
是使熔融金屬與鐵基體反應(yīng)而產(chǎn)生合金層,從而使基體和鍍層二者相結(jié)合。熱鍍鋅是先將鋼管進行酸洗,為了去除鋼管表面的氧化鐵,酸洗后,通過氯化銨或氯化鋅水溶液或氯化銨和氯化鋅混合水溶液槽中進行清洗,然后送入熱浸鍍槽中。熱鍍鋅具有鍍層均勻,附著力強,使用壽命長等優(yōu)點。
冷鍍鋅就是電鍍鋅,鍍鋅量很少,只有10-50g/m2,其本身的耐腐蝕性比熱鍍鋅管相差很多。正規(guī)的鍍鋅管生產(chǎn)廠家,為了保證質(zhì)量,大多不采用電鍍鋅(冷鍍)。只有那些規(guī)模小、設(shè)備陳舊的小企業(yè)采用電鍍鋅,當(dāng)然他們的價格也相對便宜一些。目前建設(shè)部已正式下文,淘汰技術(shù)落后的冷鍍鋅管,今后不準用冷鍍鋅管作水、煤氣管。