ABS HI-100H LG化學(xué)
原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 熔體流動速率 | 200℃/5kg | ASTM D-1238 | 1 | g/10min |
熔體流動速率 | 220℃/10kg | ASTM D-1238 | 11 | g/10min | |
熔體流動速率 | 230℃/3.8kg | ASTM D-1238 | 3 | g/10min | |
物理性能 | 比重 | ? | ASTM D-792 | 1.02 | g/cc |
成型收縮率 | ? | ASTM D-955 | 0.4-0.7 | % | |
機(jī)械性能 | 拉伸強(qiáng)度 | 50mm/min | ASTM D-638 | 380 | kg/cm2 |
拉伸模量 | 1mm/min | ASTM D-638 | 17200 | kg/cm2 | |
屈服伸長率 | 50mm/min | ASTM D-638 | 6 | % | |
斷裂伸長率 | 50mm/min | ASTM D-638 | 25 | % | |
彎曲強(qiáng)度 | 15mm/min | ASTM D-790 | 595 | kg/cm2 | |
彎曲模量 | 15mm/min | ASTM D-790 | 19300 | kg/cm2 | |
IZOD缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D-256 | 52 | kg.cm/cm | |
IZOD缺口沖擊強(qiáng)度 | 1/4" -30℃ | ASTM D-256 | 31 | kg.cm/cm | |
IZOD缺口沖擊強(qiáng)度 | 1/8" 23℃ | ASTM D-256 | 51 | kg.cm/cm | |
IZOD缺口沖擊強(qiáng)度 | 1/8" -30℃ | ASTM D-256 | 34 | kg.cm/cm | |
洛氏硬度 | ? | ASTM D-785 | 94 | R-scale | |
熱性能 | 熱變形溫度 | 18.5kg/cm2 1/4"退火 | ASTM D-648 | 92 | ℃ |
熱變形溫度 | 18.5kg/cm2 1/4"未退火 | ASTM D-648 | 85 | ℃ | |
熱變形溫度 | 4.6kg/cm21/4"退火 | ASTM D-648 | 92 | ℃ | |
熱變形溫度 | 4.6kg/cm21/4" 未退火 | ASTM D-648 | 89 | ℃ | |
維卡軟化點(diǎn) | 5kg, 50℃/h | ASTM D-1525 | 93 | ℃ | |
阻燃等級 | 1/8" | UL94 | HB | calss | |
阻燃等級 | 1/16" | UL94 | HB | calss |