適用于焊接19 Cr 10 Ni牌號(hào)鋼種的超低碳含量不銹鋼焊條。其也適用于焊接成分類似的穩(wěn)定化不銹鋼,母材需要滿足足夠抗蠕變性時(shí)除外。
分類: | E 19 9 L R 1 2, EN ISO 3581-A, E308L-17, SFA/AWS A5.4, E308L-17, CSA W48, 1.4316, Werkstoffnummer |
認(rèn)證: | Stainless, ABS, EN 13479, CE, CSA W48: E308L-17, CWB, 30.039.02, DB, VL 308 L, DNV-GL, 2.0-4.0 mm, NAKS/HAKC, UNA 272580, Seproz, 00792, VdTüV |
Approvals are based on factory location. Please contact ESAB for more information.
Alloy Type: | Austenitic CrNi |
Coating Type: | Acid Rutile |
Ferrite Content: | FN 3-10 |
Welding Current: | DC+, AC |
ISOAs welded | |
Impact Value | Testing Temperature |
70 J | 20 °C |
49 J | -60 °C |
ISOAs welded | ||
Elongation | Tensile Strength | Yield Strength |
45 % | 580 MPa | 430 MPa |
AWSAs welded | ||
Elongation | Tensile Strength | Yield Strength |
- | - | - |
Fusion time per electrode at 90% I max | kg weld metal/kg electrodes | Number of electrodes/kg weld metal | 安培 | 熔敷率 | 電壓 V | 直徑 |
24 sec | 0.55 kg | 240 | 35-45 A | 0.6 kg/h | 27 V | 1.6 x 300 mm |
29 sec | 0.55 kg | 160 | 35-65 A | 0.8 kg/h | 29 V | 2.0 x 300 mm |
36 sec | 0.55 kg | 99 | 50-90 A | 1.1 kg/h | 31 V | 2.5 x 300 mm |
54 sec | 0.60 kg | 49 | 70-130 A | 1.4 kg/h | 31 V | 3.2 x 350 mm |
60 sec | 0.60 kg | 33 | 90-180 A | 2.0 kg/h | 32 V | 4.0 x 350 mm |
60 sec | 0.60 kg | 20 | 140-250 A | 3.0 kg/h | 33 V | 5.0 x 350 mm |