Atom Arc 8018 electrodes deposit 1% Ni weld metal. They are used primarily to weld high-tensile steels in the 70-80 ksi (483-552 MPa) tensile strength range, especially where notch toughness at temperatures as low as -40°F (-40°C) is required.
焊縫金屬分析Condition | Impact Value | Stress Relieved Testing Temp | Stress Relieved Testing Time | Testing Temperature |
Stress Relieved | 129 ft-lb | 1150 °F | 8 hr | -20 °F |
Stress Relieved | 115 ft-lb | 1150 °F | 8 hr | -40 °F |
Condition | Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength |
Stress Relieved | 30 % | 1150 °F | 8 hr | 81 ksi | 70 ksi |
安培 | 效率 (%) | 最佳電流 | 熔敷率 | 直徑 |
70-100 A | 66.3 % | 90 A | 0.8 kg/h | 2.4 mm |
90-160 A | 71.6 % | 120 A | 1.2 kg/h | 1/8 in. |
90-160 A | 70.9 % | 140 A | 1.2 kg/h | 1/8 in. |
130-220 A | 75 % | 140 A | 1.1 kg/h | 4.0 mm |
130-220 A | 73.5 % | 170 A | 1.7 kg/h | 4.0 mm |
200-300 A | 76.4 % | 200 A | 2.2 kg/h | 3/16 in. |
200-300 A | 74.6 % | 250 A | 2.4 kg/h | 3/16 in. |